Cold Heading Cracking Causes
Three cold-heading crack causes: material defects (inclusions, seams), excess deformation (heading ratio), tooling and lubrication; 45° or ring cracks point to deformation first.
Troubleshooting order
- Locate by crack position and angle → station
- Metallography for inclusions and decarburisation
- Check heading ratio (≤4.5 for pan heads)
- Check die radii and lubricant coating
Standards basis
Basis: "Cold Heading Technology of Metals" and "Practical Cold Extrusion" — crack modes (longitudinal, end, laps) analysed by monograph criteria for material and die conditions.
FAQ
What is the MOQ for Cold Heading Cracking Causes?
Stock items ship in small batches; custom parts are quoted per tooling and process — the quotation is authoritative.
What is the lead time for Cold Heading Cracking Causes?
Samples in 1 day for stock, volume 7–15 days; new tooling samples in 3–7 days.
Can cold heading cracking causes be made to drawing?
Yes — process review within 48 h, samples in 3–7 days, full first-article inspection before volume.
Are inspection reports available?
Dimensional reports ship per batch; salt-spray, pull-out and mechanical data is published and quotable on the test-data pages.
Need a spec check or 1-day sample?
Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).
Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))