Skip to content

Galvanic corrosion aluminum steel

Galvanic corrosion: steel–aluminium differ by ≈0.8 V, so aluminium corrodes continuously when electrolyte (rain, condensate) is present. Cut the electrolyte or the potential.

By YF Zhichengjia engineering

Galvanic corrosion aluminum steel

Three conditions

  • Potential difference measurable from ≈0.15 V
  • Electrolyte bridge (rain, salt fog, condensate)
  • Small anode / large cathode geometry is worst

Three fixes

(1) Zinc-nickel or Dacromet bolts (lower potential), (2) plastic/elastomer isolating washers, (3) drainage plus sealing to stop pooling — combined, most robust.

Standards basis

Basis: GB/T 3098.10-1993 (bolts, screws, studs and nuts of non-ferrous metals) — aluminium property classes and galvanic pairing follow this system.

FAQ

Stainless on aluminium?
Yes, but ΔV ≈0.5 V remains — isolate and drain outdoors.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))