Skip to content

Heat Treatment Effect on Strength

How heat treatment drives strength: quench-and-temper lifts medium-carbon steel from 400 to 800–1200 MPa; higher temper temperature means more toughness at lower strength.

By YF Zhichengjia engineering

Heat Treatment Effect on Strength

Class–treatment map

ClassProcessTemper
8.8 (≤M16)QT or normalizedLow-temperature temper
10.9QT≈425 °C
12.9QT≈425 °C (minimum)

Standards basis

Basis: "Essential Theory for Heat-Treatment Engineers" plus GB/T 3098.1-2010 — hardenability and tempering effects follow the monograph; acceptance values follow the standard.

FAQ

What is the MOQ for Heat Treatment Effect on Strength?
Stock items ship in small batches; custom parts are quoted per tooling and process — the quotation is authoritative.
What is the lead time for Heat Treatment Effect on Strength?
Samples in 1 day for stock, volume 7–15 days; new tooling samples in 3–7 days.
Can heat treatment effect on strength be made to drawing?
Yes — process review within 48 h, samples in 3–7 days, full first-article inspection before volume.
Are inspection reports available?
Dimensional reports ship per batch; salt-spray, pull-out and mechanical data is published and quotable on the test-data pages.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))