Skip to content

Galvanic Corrosion Protection

Galvanic-corrosion protection: metal pairs over ~0.25 V potential difference accelerate attack in electrolyte. Potential-difference table, a checking tool and three countermeasures below.

Common potential differences

PairΔV (V)Risk and countermeasure
Steel bolt – aluminium≈0.8Al side corrodes → zinc-nickel bolt + isolating washer
Stainless – aluminium≈0.5Controllable → avoid electrolyte pooling + insulation
Copper – aluminium≈0.4Hazardous → tin-plated transition + sealing
Titanium – aluminium≈0.7Ti is cathodic → insulating sleeve + washer
Source: Seawater galvanic series (reference values)

Specs, MOQ and lead time

Size range
Precision fasteners: micro screws M0.6–M3, insert screws M1.4–M8, threaded inserts M2–M12 / 10-24 to 1/2-13, bolts, nuts and washers M2–M16
Stock items
Retained-stock SKUs ship from stock; see the stock page for the current list
MOQ
Small quantities for stock items; custom parts quoted per tooling and process
Tiered pricing
Three tiers: sampling / small batch / volume production
Lead time
Samples in 1 day for stock; volume 7–15 days; new tooling samples in 3–7 days
Packing & OQC
Packed to customer spec; shipment with inspection report (dimension / visual / salt spray / pull-out as required)

FAQ

Stainless screws on aluminium?
Yes — cut the electrolyte path: seal, insulate, drain.
How does the galvanic checker work?
Enter both materials and the environment; it returns ΔV and coating advice.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))