Skip to content

Hydrogen embrittlement prevention

Hydrogen-embrittlement prevention: plated parts above grade 10.9 can crack under sustained stress; bake at 190–210 °C for 4 h within 4 hours of plating.

By YF Zhichengjia engineering

Hydrogen embrittlement prevention

Hydrogen sources

  • Over-pickling
  • Electroplating hydrogen
  • Cathodic e-coat and cleaning residues

Verification

Verify by slow-strain-rate or sustained-load sampling per batch; the safer route is Dacromet, which avoids electroplating hydrogen entirely.

Standards basis

Basis: GB/T 3098.17-2000 (pre-loading parallel bearing-surface test for hydrogen embrittlement) — batch sampling clamps to specified preload, holds, then unloads and inspects.

FAQ

Coating for grade 12.9?
Dacromet, or zinc-nickel with strict bake-out — avoid plain zinc.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))