Skip to content

Hydrogen Embrittlement

Hydrogen embrittlement: hydrogen from pickling/plating embrittles steel under stress — risk rises sharply above grade 10.9; bake at 190–210 °C for 4 h.

Three controls

  • Process: control pickling, prefer non-cyanide plating or Dacromet
  • Bake: ≥190 °C × 4 h within 4 h of plating
  • Verify: slow-strain-rate or sustained-load testing by batch

FAQ

Can grade 12.9 be plated?
Yes but risky — prefer Dacromet or zinc-nickel with strict bake-out.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))