Stainless Galling Causes

Why stainless galls: the oxide film on austenitic stainless breaks and reforms under friction, causing local cold welding — worst with slow, high-torque drive-in.

By YF Zhichengjia engineering

Stainless Galling Causes

Four fixes

  • DLC coating (friction −50%+)
  • Anti-seize paste (Cu/Ni based)
  • Faster drive-in (less friction time)
  • Dissimilar pairing (A2 bolt + A4 nut)

Standards basis

Basis: BS EN ISO 3506-1:2009 (mechanical properties of corrosion-resistant stainless fasteners — bolts, screws, studs) — steel groups (A1/A2/A4) and property grades (50/70/80) follow this standard.

FAQ

How to free a galled fastener?
Heat expansion or impact torque — prevention beats rescue.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))