Pain points

  • Loosening under road excitation (10–500 Hz): tray joints and e-drive mounts lose preload continuously.
  • Galvanic attack: aluminium trays against steel bodies, magnesium housings against steel fasteners (ΔV >0.25 V accelerates corrosion).
  • Sealing failures: leaks at pack joints under IP67 requirements trip insulation alarms.
  • Lightweighting at cost: steel-to-aluminium is the direction, but steel bolts are galvanically wrong on aluminium.

Selection table

LocationRecommended mixKey points
Pack tray jointsPre-applied adhesive screws + flange bearing facesRoad-excitation locking + lower embedment
Al tray to steel bodyZn-Ni coating + plastic isolating washersIsolation beats simply thickening coatings
Magnesium e-drive housingsHigh-strength aluminium bolts + head sealantSmall Al-Mg gap + physical isolation cuts the cell
Pack sealingBonded seals + torque-controlled assemblyPre-coated rivet nuts/blind rivets reach IP68
Chassis sheetRivet nuts, rivet bolts, blind rivetsSingle-side install; clinch earth terminals for earthing
Cast threadsMoulded-in / self-tapping insertsInserts bring cast threads above grade 8.8

Test data

  • Lifting sleeve: −60% cost, <4 min cycle, 98% utilisation with continuous grain flow (better stress-fracture resistance).
  • ZT68 bolts: tensile mean ≈629 MPa (5 samples), wedge 627–639 MPa, breaking torque ≥25 N·m, 150 °C×12 h and 60-day salt spray passed.
  • Coatings: Zn-Ni 720 h+ to white rust; Dacromet 1000 h+ hydrogen-free; electroplated parts ≥1000 MPa (HRC 32) must be baked.
  • Locking: adhesive + prevailing torque per GB/T 3098.9; torque window re-set after measuring the actual stack per GB/T 16823.3.

Application cases

  • Battery-pack lifting sleeve: cold heading replaced machining in volume (−60% cost, 5× output) — full comparison on the case-studies page.
  • Aluminium lifting sleeves, ZT68 bolts and adhesive locking screws ship in volume; import substitutions verified line by line.
  • E-powertrain and chassis: clinch parts fasten and earth thin sheet/castings; structural aluminium sleeves cold-forged instead of CNC — cost and cycle both down.

FAQ

What goes into pack fastener acceptance?
Torque window (measured friction), locking (GB/T 3098.9), coating thickness and salt spray (GB/T 5267.1 / 10125), sealing class (IP67/68), hydrogen sampling (GB/T 3098.17).
Steel bolts straight onto aluminium trays?
Short term yes, but aluminium corrodes fast in electrolyte; use Zn-Ni + isolation, or switch to ZT68 aluminium bolts (galvanic-compatible).

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))