Pain points

  • Thread stripping: soft Al/Mg threads carry poorly and crush under repeated assembly.
  • Porosity leaks: pores cluster at thickness changes — threads landing in porous zones leak.
  • Galvanic attack: magnesium against steel fasteners corrodes fast — white rust and thread destruction.
  • Tooling economics: every added machining step dilutes the casting cost advantage.

Selection table

LocationRecommended mixKey points
High-volume threaded holesMoulded-in insertsFormed in one shot, lowest unit cost
Service/prototype partsSelf-tapping insertsNo tapping; restores stripped holes
Standard-hole repairWire thread insertsInstalls into a standard drilled hole, restoring strength
Process-hole sealingSealing plugs (expansion / press-fit / standard)Three types by hole size and pressure
Plain holesThread-rolling tapping screwsRolled threads with strength and locking built in
Magnesium jointsHigh-strength aluminium bolts + head sealantSmall Al-Mg gap + physical isolation

Test data

  • Insert strength: carbon/stainless inserts bring cast threads above grade 8.8 — the direct fix for weak light-alloy threads.
  • Leak control: route threads away from porous zones + sealant + tighten to porosity-safe clamp loads (all three; sealant alone does not fix crush).
  • Galvanic: the Al-Mg potential gap is small, and head-face adhesive adds isolation — cutting the cell at its root.
  • Selection order: high volume with tooling access → moulded-in; service/prototype → self-tapping; standard-hole repair → wire inserts.

Application cases

  • Housing thread conversions: moulded-in and self-tapping routes in volume — full case on the case-studies page.
  • Sealing plugs: expansion, press-fit and standard types matched to process holes.
  • Lightweight joints: ZT68 aluminium bolts measured ≈629 MPa mean tensile, galvanically compatible with aluminium structures.

FAQ

Moulded-in or post-install?
High volume with tooling access → moulded-in; service and prototypes → post-install. Self-tapping inserts also restore stripped holes.
Is sealant enough for cast-thread leaks?
No — porosity is the root cause: route threads away from porous zones, add sealant and control clamp loads together.

Need a spec check or 1-day sample?

Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).

Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))