Fastener Property Class Comparison
Property class comparison: carbon steel 4.8–12.9, stainless A2/A4-50~80, aluminium 600 MPa — strength and use. Conclusion: structural joints start at 8.8.
Table
| Class | Tensile (MPa) | Yield (MPa) | Typical use |
|---|---|---|---|
| 4.8 | 400 | 320 | Light sheet duty |
| 8.8 | 800 | 640 | General structures |
| 10.9 | 1000 | 900 | High preload |
| 12.9 | 1200 | 1080 | Tools / dies |
| A2-70 | 700 | 450 | Corrosion duty |
| A4-80 | 800 | 600 | Corrosion + strength |
| ZT68 Al | 600 | 540 | Lightweight aluminium |
| Source: GB/T 3098.1 / 3098.6 and in-house tests | |||
FAQ
What is the MOQ for Fastener Property Class Comparison?
Stock items ship in small batches; custom parts are quoted per tooling and process — the quotation is authoritative.
What is the lead time for Fastener Property Class Comparison?
Samples in 1 day for stock, volume 7–15 days; new tooling samples in 3–7 days.
Can fastener property class comparison be made to drawing?
Yes — process review within 48 h, samples in 3–7 days, full first-article inspection before volume.
Are inspection reports available?
Dimensional reports ship per batch; salt-spray, pull-out and mechanical data is published and quotable on the test-data pages.
Need a spec check or 1-day sample?
Send us your drawing, spec or part code. We reply the same day on stock, MOQ, tiered pricing and lead time (1-day sampling for stock; volume 7–15 days).
Call directly: +86 135-1036-9429(Mr. Zhang (Engineering & Sales Director)) · +86 135-6073-0094(Ms. Fan (Sales Manager))